Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Recycloblend " in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
...able material in end-of-life cars. By 2015, some 95% of the plastics are to be recycled and fed back into automotive applications. As a result, increased use is already being made of polyolefins today. Additives such as Recyclostab or Recycloblend provide support in the recycling of bumpers, battery cases and petrol tanks, making it possible to achieve virtually the same properties as in virgin material. Figure 5 compares the properties of painted bumpers in new material with those made of recyc...
Kunststoffe international, 2005-11-21, Stabilization - Doping for Recyclates
...the case of the non-restabilized regrind material, a reduction in the stabilizer content can be detected immediately after processing. Artificial Weathering Following the tests on the heat resistance-oriented restabilization, the variant with 1 % Recycloblend 660 was used as the basis for the heat ageing trials. To make the PP regrind mixture suitable for outdoor applications, it was mixed with, among other things, various amounts of Tinuvin 791. Fig. 5 illustrates the influence of the weatheri...
Kunststoffe international, 2015-12-17, Improving the Quality of Recycled Materials
...al obtained from garden chairs to such an extent that it can be re-used in the same application (Fig. 2) [3]. Particularly high stability is achieved in this case if long-term stabilization with antioxidants/HALS is augmented with a repair system (Recycloblend 660, see below) to deactivate the filler.Reactive Molecules and Repair SystemsStabilizers can generally only retain their existing properties for a certain length of time, albeit an extended one. It is therefore not possible to heal a dam...
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.